One can use either an EDS or WDS system to produce an element map.
The best element maps are acquired using a WDS system on an electron microprobe, but the trade-off in using the spectrometers is longer acquisition time.
we implemented an additional driving force resulting from the difference in the stored energy between the grains/phases which takes only effect if one of the grains/phases has a stored energy of 0
For doing so, you have to define recrystallisation for both phases in the phase input section of the MICRESS input file